Color (A+B) Amber
Viscosity (mixed) 500 cps
Mix Ration (by volume) 2:1
Pot Life 100 grams @ 77°F 30 mins
Linear Coefficient of Shrinkage .0043
Absorption ASTM D-570 24 hrs 0.84 %
Shrinkage ASTM C-883 Passes
Gel Time ASTM C-881 45 mins
Heat Deflection Temperature
ASTM D-648 120°F
Bond Strength ASTM C-882 2 days 2,580 psi
14 days 3,735 psi
Compressive Strength @73°F
ASTM D-695 7 days 12,385 psi
Tensile Strength @ 73°F 14 days
ASTM D-638 7,168 psi
Flexural Strength
ASTM D-790 8,700 psi
Shear Strength
ASTM D-732 8,500 psi
To gravity feed cracks:
Pour neat HT-500 LV into vee-notched crack. Continue placement until completely filled. Seal underside of slab prior to filling if cracks reflect through.
To pressure-inject cracks:
Use automated injection equipment of manual methods. Set appropriate injection ports based on system used. Seal ports and cracks with HI-TECH Structural Gel or HI-TECH Structural Gel Fast. When the epoxy adhesive seal has cured, inject HT-500 LV with steady pressure. Consult Technical Service for additional information.
To seal slabs:
Spread neat HT-500 LV over slab. Allow penetration. Remove excess to prevent surface film. Seal interior slabs and above grade exterior slabs only.
For use as an epoxy mortar:
Prime prepared surface with neat HT-500 LV. Place prepared epoxy mortar before primer becomes tack-free. Place the epoxy mortar using trowels. Compact and level with vibrating screed or trowels. Finish with finishing trowel. Exterior application may darken with ultra violet exposure.