Rebuilding control joints
Shallow spalls on bridge decks
Traffic area spalls & crack repairs
Grade matching
Floor repair
Stops additional damage
Fill & repair spall before coating
Used to “knit” cracked slabs |
|
Meets USDA and FDA Requirements
Cures from -20° F to 130° F.
“Drive-Over” in 10 to 15 minutes
Produces High Strength Quickly
Slightly Flexible
Self-leveling
Self Priming
Fast initial set; rapid gain to ultimate strengths.
|
Viscosity (Mixed)
Hardness, durometer (ASTM D2240)
Tensile Strength, PSI (ASTM D412) -
Tear Strength (ASTM D624)
Elongation % (ASTM D412) -
Compressive Strength (neat)
(with sand)
Bond Strength ASTM 882-99 |
250 cps
60A
3700
-lb/mil 460
7% to 9%
3400 psi
4500 psi
3450 |
22 oz. & 56 oz. Cartridges
1 Gallon Kit (with proportioning chambers)
2 Gallon, 5 Gallon, 10 Gallon Kits